Influence of thermal cycles in water on flexural strength of laboratory-processed composite resin
F Kawano1, T Ohguri, T Ichikawa
1Department of Removable Prosthodontics, The University of Tokushima, School of Dentistry, Tokushima, Japan. fumiaki@dent.tokushima-u.ac.jp
Abstract:
Recently a new generation of laboratory-processed composite resins containing submicron glass fillers was introduced, with claims of high strength. The purpose of this study was to evaluate the effect of thermal cycling in water on the flexural strength and hardness of several laboratory composite systems. The flexural strength of the new laboratory processed composite resins (Artglass [AG], Targis [TR] and Estenia [ES]) was significantly higher than that of conventional resins (Dentacolor [DC] and Cesead II [CS]). Thermocycling caused a reduction of the flexural strength but not a reduction of the hardness for most of materials tested. It was concluded that thermocycling affected the properties of the laboratory-processed hybrid type composite resin, ES, AG and TR. However, the changes of these properties were smaller than those of microfine type composite resin DC. Thus, ES, AG and TR may maintain better properties during service compared with DC.
Related Concept Videos
Flexural Stress
Hooke's Law states that within the material's elastic limits, stress is directly proportional to strain. In a member experiencing a bending moment, the strain at any point is relative to its distance...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...
Fatigue
Residual Stresses in Bending