Clinical performance of resin-retained fixed partial dentures bonded with a chemically active luting cement
Related Experiment Video
Updated: Oct 3, 2026

Standardized Protocol to Evaluate the Effect of Surface Treatments, Luting Cements, and Thermocycling on PEEK–Composite Bond Strength
Published on: June 9, 2026
1Department of Conservative Dentistry, University of Wales College of Medicine, Dental School, Cardiff, United Kingdom.
Abstract:
A clinical study was undertaken to review resin-retained fixed partial dentures bonded with a chemically active luting cement during a 4-year period. One hundred thirty-seven fixed partial dentures were reviewed of which five had failed because of a nonbonding failure (esthetics, trauma, fracture) and 47 (36%) had failed after a bonding failure, of which 72% were rebonded. The mean time of failure was 10.9 months (SD 9.8). The failure rate appeared to be affected by position, use of a rubber dam, and the fixed partial denture design, although no one factor reached conventional statistical significance.