Nanoindentation and storage of teeth
Related Experiment Video
Updated: Aug 18, 2026

Characterization Of Multi-layered Fish Scales (Atractosteus spatula) Using Nanoindentation, X-ray CT, FTIR, and SEM
Published on: July 10, 2014
Stefan Habelitz1, Grayson W Marshall, Mehdi Balooch
1Department of Preventive and Restorative Dental Sciences, University of California, San Francisco, CA 94143 0758, USA. shabeli@itsa.ucsf.edu
Abstract:
This study determined changes in nanomechanical properties of dentin and enamel during storage in deionized water, calcium chloride buffered saline solution and Hank's balanced salts solution (HBSS). Atomic force microscopy based nanoindentation showed that storing teeth in deionized water or CaCl(2)-solution resulted in a large decrease in elastic modulus and hardness. At 1 day a decrease in the mechanical properties values of up to 20% and 30% was observed for enamel and dentin, respectively. After 1 week, mechanical properties dropped below 50% of their starting values, which is attributed to a demineralization process during storage. In contrast, storing teeth in HBSS did not significantly alter the mechanical properties for a time interval of 2 weeks. The use of HBSS for storage of samples from teeth is recommended.
Related Concept Videos
Teeth
In the bud stage, the tooth germ (an aggregation of cells) starts to form in the developing jawbone. During the cap stage, the tooth germ differentiates into enamel organ, dental papilla, and dental sac, which will later develop into the tooth's enamel, dentin and...
Tooth Anatomy
The Crown, Neck, and Root
The visible part of the tooth is referred to as the crown. It's covered by enamel, the hardest substance in the human body. The crown is uniquely shaped for each type of tooth, allowing for different functions such as cutting, tearing, or grinding food.