Related Experiment Video
Updated: Sep 30, 2026

Aerosol-assisted Chemical Vapor Deposition of Metal Oxide Structures: Zinc Oxide Rods
Published on: September 14, 2017
Light-assisted chemical deposition of highly (0001) oriented zinc oxide film
1Department of Inorganic Chemistry, Osaka Municipal Technical Research Institute, 1-6-50 Morinomiya, Joto-ku, Osaka 536-8553, Japan. izaki@omtri.city.osaka.jp
Abstract:
Highly (0001) oriented zinc oxide (ZnO) films of smooth layer type and hexagonal columns have been prepared on quartz glass substrates at temperature as low as 323 K by UV light assisted chemical deposition from an aqueous solution containing hydrated zinc nitrate and dimethylamine-borane (DMAB).
More Related Videos
08:18Synthesis and Characterization of High c-axis ZnO Thin Film by Plasma Enhanced Chemical Vapor Deposition System and its UV Photodetector Application
Published on: October 3, 2015
08:14Improved Heterojunction Quality in Cu2O-based Solar Cells Through the Optimization of Atmospheric Pressure Spatial Atomic Layer Deposited
Zn1-xMgxO
Published on: July 31, 2016