[Measurement and differentiation method of carbon in municipal solid waste incineration (MSWI) bottom ash using
L Quilici1, A Praud Tabaries, J Benaim
1Laboratoire de recherche en chimie marine des organométalliques, Université de Toulon et du Var, La Garde, France.
Abstract:
In this study, Differential Scanning Calorimetry (DSC) is applied to speciation and evaluation of carbon in Municipal Solid Waste Incineration (MSWI) bottom ash. This innovative recognition approach highlights and quantifies different types of carboned materials in bottom ash: Labile Organic Carbon (LOC) and Refractory Carbon (RC). The Labile Organic Carbon contains small molecules unburnt or decomposed and volatile. This organic material (LOC) is oxidized at medium temperatures (between 300 and 325 degrees C). The Refractory Carbon contains Elementary Carbon (EC) and Resistant Organic Carbon (ROC) in the form of complex molecules of high molecular weight. This is oxidized at high temperatures (between 435 and 470 degrees C).
More Related Videos
Related Concept Videos
Sample Preparation for Analysis: Advanced Techniques
Acid digestion with strong acids is commonly used to dissolve inorganic materials that are insoluble (do not dissolve) in water. This method can be useful for...
Constant Volume Calorimetry
Atomic Absorption Spectroscopy: Lab
Solutions containing organic solvents, such as low-molecular-mass alcohols, esters, or ketones, enhance absorbances by increasing nebulizer...
Volatilization