Related Experiment Video
Updated: Aug 8, 2026

10:27
The Evolution of Silica Nanoparticle-polyester Coatings on Surfaces Exposed to Sunlight
Published on: October 11, 2016
[XPS and AES studies of the Ni-P-SiO2 composite coating]
Guang Pu Xue Yu Guang Pu Fen Xi = Guang Pu
|August 30, 2003
Abstract:
The morphology and composition of the composite coating of the Ni-P-SiO2 were analyzed by using the methods of SEM, AES and XPS. The results show the composite deposit is very smooth, uniform and good appearance. The coating is approximately 6.40 microns thick and has stronger corrosion resistance. The relative atomic percent contents of the coating is Ni 74.56%, P 12.38%, Si 2.77%, O 6.65% and Fe 2.32%.