Short-term natural weathering of MSWI bottom ash as a function of particle size

J M Chimenos1, A I Fernández, L Miralles

  • 1Department of Chemical Engineering and Metallurgy, University of Barcelona, Martí i Franquès 1, 08028 Barcelona, Spain. chimenos@material.qui.ub.es

Related Concept Videos

Deleterious Substances in Aggregate01:25

Deleterious Substances in Aggregate

Deleterious substances in aggregates can be detrimental to the quality and durability of concrete. These substances include organic impurities like loam, which interfere with cement hydration and are usually present in the sand. These prevent a good bond between aggregate and cement paste. Organic impurities can be detected using the colorimetric test, where the darkness of a solution after agitation indicates the level of organic content.
Another type of impurity is clay and fine material that...
Design Example: Managing Concrete Workability01:14

Design Example: Managing Concrete Workability

This example deals with managing the workability of concrete for a raft foundation project under hot weather conditions. Workability is crucial for ensuring the concrete is easy to place, compact, and finish. In this scenario, a slump test — a common method to measure the workability of fresh concrete — initially indicated low workability. This was attributed to the rapid water loss from the concrete mix, exacerbated by the high temperatures causing the course aggregates to heat up.
To address...
Factors Affecting Workability01:24

Factors Affecting Workability

The workability of concrete is a critical characteristic that influences the ease of mixing, handling, and finishing the concrete. It is affected by several factors including water content, aggregate properties, and admixtures like air entrainment. Water plays a fundamental role as it lubricates the concrete mix, facilitating easier movement and placement. However, the water requirement varies depending on the texture and shape of aggregates. Finer particles and angular, rough-textured...
Unsoundness of Aggregate due to Volume Change01:26

Unsoundness of Aggregate due to Volume Change

Unsoundness in aggregates due to volume changes is primarily caused by the physical alterations aggregates undergo, such as freezing and thawing, thermal changes, and wetting and drying. Unsound aggregates, when subjected to these changes, result in volume change upon disintegration. This, in turn, contributes to the deterioration of concrete, including scaling, pop-outs, and cracking. Particular types of aggregates, such as porous flints, cherts, and those containing clay minerals, are...
Porosity and Absorption of Aggregate01:20

Porosity and Absorption of Aggregate

Aggregates contain pores of varying sizes; while some are completely enclosed within the particles, others open onto the surface, allowing water to penetrate. The porosity of aggregates is a major factor contributing to the overall porosity of concrete, given that aggregates constitute about three-quarters of concrete's volume.
When all pores in an aggregate are filled with water, the aggregate is considered saturated and surface-dry. If left in dry air, water will evaporate until the aggregate...
Fineness of Cement01:15

Fineness of Cement

The fineness of cement directly influences the rate of hydration, as the hydration begins at the surface of the cement particles. In addition to hydration, the fineness of cement is vital for various properties of concrete including workability, gypsum requirement, and long-term behavior. The fineness of cement is represented in terms of the specific surface of cement which is typically measured in square meters per kilogram, with several methods available for this determination.
Direct...