An evaluation of the standardized chipping hammer test specified in ISO 8662-2
R G Dong1, T W McDowell, D E Welcome
1Engineering & Control Technology Branch, National Institute for Occupational Safety and Health, 1095 Willowdale Road, Morgantown, WV 26505, USA. rkd6@cdc.gov
Objectives:
Prolonged exposure to severe chipping hammer vibration may cause hand-arm vibration syndrome. A reliable test method is required to select appropriate tools and assist in the development of better chipping hammers. In the present study, the ISO standardized test method (ISO 8662-2, 1992) was examined through an investigation of the vibration characteristics of chipping hammers operating on the energy absorber specified in the standard.
Methods:
The energy absorber and test setup were designed and constructed based on those specified in the standard. The experiment employed six subjects and used two pneumatic chipping hammers and three different feed forces (50, 100 and 200 N). The subject posture was the same as that specified in the standard.
Results:
The vibration emission at the tool dominant frequency (or air blow rate) generally declined with an increase in feed force, thus decreasing the frequency-weighted accelerations. The increase in feed force, however, resulted in an increase in the unweighted vibration emission at high frequencies. The chipping hammer vibration emission operating on the energy absorber at the high feed force (200 N) was inconsistent.
Conclusions:
The measurement method has a good repeatability except at a high feed force. The feed force has a significant effect on the vibration emission. The single feed force specified in the standard may not be sufficient to test the tool behaviors. Multiple levels of feed force should be used for the chipping hammer test. Doing so may provide a more appropriate basis for tool screening.
Related Concept Videos
Non-destructive Tests for Concrete Strength
Toughness and Hardness of Aggregate
Vebe Test
To conduct the test, concrete is placed into the slump cone. The concrete is filled in layers and...
Compacting Factor test
The procedure begins by placing concrete into the upper hopper without any compaction. Once filled, the bottom door of this hopper is opened,...
Slump Test
Concrete is poured into the mold in three layers to conduct the test. Each layer is compacted 25 times with a steel tamping rod, which has a five-eighths-inch diameter and a rounded end, to ensure even distribution and eliminate...