Related Experiment Video
Updated: Aug 24, 2026

Micromechanical Tension Testing of Additively Manufactured 17-4 PH Stainless Steel Specimens
Published on: April 7, 2021
The influence of specimen attachment and dimension on microtensile strength
A A El Zohairy1, A J de Gee, N de Jager
1Department of Dental Materials Science, Academic Center for Dentistry Amsterdam (ACTA), Louwesweg 1, 1066 EA Amsterdam, the Netherlands.
Abstract:
The higher microtensile bond strength values found for specimens with a smaller cross-sectional area are often explained by the lower occurrence of internal defects and surface flaws. We hypothesized that this aberrant behavior is mainly caused by the lateral way of attachment of the specimens to the testing device, which makes the strength dependent on the thickness. This study showed that composite bars of 1x1x10, 1x2x10, and 1x3x10mm attached at their 1-mm-wide side (situation A) fractured at loads of the same magnitude, as a result of which the microtensile strength ( micro TS), calculated as F/A (force at fracture/cross-sectional area), significantly increased for specimens with decreasing thickness. Attachment at the 1-, 2-, or 3-mm-wide side (situation B) resulted in equal micro TS values (P > 0.05). Finite element analysis showed different stress patterns for situation A, but comparable patterns for situation B. Both situations showed the same maximum stress at fracture.
Related Concept Videos
Tensile Strength Considerations of Concrete
The dimensions and shape of a concrete specimen also...
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used to...
Stress-Strain Diagram
Relation Between Tensile Strength and Compressive Strength of Concrete
Bonding and Strength of Aggregate
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...