Release of silica, calcium, phosphorus, and fluoride from glass ionomer cement containing bioactive glass
Helena Yli-Urpo1, Pekka K Vallittu, Timo O Närhi
1Department of Prosthetic Dentistry and Biomaterials Research, Institute of Dentistry, University of Turku, Lemminkäisenkatu 2, 20520, Finland. helena.yli-urpo@utu.fi
Abstract:
The aim of this study was to examine the release of silica (Si), calcium (Ca), phosphorous (P), and fluoride (F) from conventional glass ionomer cement (GI) and resin-modified glass ionomer cement (LCGI), containing different quantities of bioactive glass (BAG). Further aim was to evaluate in vitro biomineralization of dentine. The release of Si increased with the increasing immersion time from the specimens containing BAG, whereas the amount of Ca and P decreased indicating in vitro bioactivity of the materials. LCGI with 30wt% of BAG showed highest bioactivity. It also showed CaP-like precipitation on both the surface of the test specimens and on the dentin discs immersed with the material. Within the limitations of this study, it can be concluded that a dental restorative material consisting of glass ionomer cements and BAG is bioactive and initiates biomineralization on dentin surface in vitro.
Related Concept Videos
Hydration of Cement
Essential Minerals for Bone Health
Calcium and Phosphorus
Calcium is a critical component of bones, especially in the form of calcium phosphate and calcium carbonate. Since the body cannot make calcium, it must be obtained from the diet. However, calcium cannot be absorbed from the small intestine without...
Biofilms
Alkali Aggregate Reaction in Concrete
Additives and Fillers in Concrete
The...
Deleterious Substances in Aggregate
Another type of impurity is clay and fine material that...