Purpose:
To compare the metal-ceramic bonding strength of different ceramic alloies.
Methods:
30 wax sheets were divided into 6 groups at random. Each group included 5 sheets. After being invested conventionally with Bellaves SH,the samples were casted and fused with porcelain.The metal-ceramic bonding strength was evaluated.
Results:
The highest bonding strength was found in Bio Herador N alloy, and then in TILITE alloy and Heraenium S alloy respectively. Bio Herador N alloy and TILITE alloy all had significant differences of the bonding strength before and after treatment (P<0.05). There was no significant differences in the bonding strength of the Heraenium S alloy after treatment (P>0.05).
Conclusion:
The bonding strength of precious metal-ceramic was higher than that of non-precious metal-ceramic.Pre-oxygen treatment can improve the metal-ceramic bonding strength of Bio Herador N alloy and TILITE alloy,but it had no effect on the metal-ceramic bonding strength of the Heraenium S alloy.
Related Concept Videos
Bonding and Strength of Aggregate
Bonding in Metals
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...
Strength and Heat of Hydration
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...