Background:
Self-etching primers are reported to produce considerable etching on flat enamel surfaces. However, little is known about the influence of different enamel surface textures. In this study the influence of grinding enamel on bond strength of two all-in-one and one two-step adhesives was investigated.
Methods:
Resin composite was bonded to the ground enamel of extracted human third molars that was reduced 0.5 mm from the buccal or lingual surfaces using either regular- or superfine-grit diamond burs with each of the three adhesives. After 24 hours in 37 degrees C water, the specimens were sectioned into slabs of 0.7 mm thickness, trimmed to an hourglass configuration, and subjected to microtensile bond strength (MTBS) testing.
Results:
For all adhesive systems, MTBS to enamel ground with a regular-grit diamond bur was not significantly different from that with a superfine-grit diamond bur. The etching patterns of these adhesives were partly varied according to the aggressiveness of the adhesives.
Conclusion:
The use of two different burs does not affect the tensile bond strength of the adhesives to enamel.
Related Concept Videos
Bonding and Strength of Aggregate
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...
Mortar Properties
Brick Durability, Strength, and Appearance