Related Experiment Video
Updated: Jul 28, 2026

Two-way Valorization of Blast Furnace Slag: Synthesis of Precipitated Calcium Carbonate and Zeolitic Heavy Metal Adsorbent
Published on: February 21, 2017
Interaction of limestone grains and acidic solutions from the oxidation of pyrite tailings
1Departamento de Edafología, EPS-CITE IIB, Cañada San Urbano, Universidad de Almería, 04120 Almería, Spain. msimon@ual.es
Abstract:
To characterise the coatings formed and to analyse element partitioning between the aqueous and solid phase, suspensions were prepared with four grain sizes of limestone and three different amounts of acidic solution from oxidized pyrite tailings. In all cases, red coatings with three different layers covered the grain surface, sealing off the acidic solution. The inner layer was composed mainly of basaluminite, the middle layer of schwertmannite, and the outer layer of gypsum and jarosite. Zn, Cd and Tl were co-precipitated by Fe and Al; As and Pb were co-precipitated almost completely by Fe; and Cu formed mainly Cu sulphates. All trace elements reached almost total precipitation at pH 6.3, but the precipitation of As and Pb tended to decrease as the pH rose. Consequently, liming should be calculated so that the soil pH does not exceed 6.3. This calculation should take into account that the armouring of the limestone grains can cause underestimations in the amount of liming material needed.
Related Concept Videos
Weak Acid Solutions
Factors Affecting Solubility
Sulfate Attack on Concrete
Sulfates from sources like soil, groundwater, or industrial effluents...
Acid Attack on Concrete
The rate at which hydrogen...
Microbial Leaching
Acid Mine Drainage