Hardness and yield strength of dentin from simulated nano-indentation tests
1Department of Metallurgical and Materials Engineering, Faculty of Engineering, Dokuz Eylul University, Bornova, Izmir, Turkey. mustafa.toparli@deu.edu.tr
Abstract:
The finite element method (FEM) is applied for studying the hardness (H) and yield strength (Y) of dentin subjected to a nano-indentation process. The nano-indentation experiments were simulated with the ABAQUS finite element software package. This test, performed with a spherical indenter, was simulated by axisymmetric finite element analysis. The load versus displacement was calculated during loading-unloading sequence for different elastic modulus (E) and yield strength. Hardness and maximum principal compressive and tensile stresses were plotted for different elastic modulus depending on yield strength. The dentin was assumed to be isotropic, homogenous and elasto-plastic. The theoretical results outlined in this study were compared with the experimental works reported in the literature and then hardness and yield strength of dentin was estimated.
Related Concept Videos
Mechanical Characteristics of Steel
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used to...
Yield Criteria for Ductile Materials under Plane Stress
The Maximum Shearing Stress Criterion, also known as the...
Non-destructive Tests for Concrete Strength
Stress-Strain Diagram - Ductile Materials
Toughness and Hardness of Aggregate