Related Experiment Video
Updated: Aug 17, 2026

Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
Effect of temporary cements on the bond strength of ceramic luted to dentin
Sahar E Abo-Hamar1, Marianne Federlin, Karl-Anton Hiller
1Department of Operative Dentistry and Periodontology, Dental School, University of Regensburg, Franz Josef Strauss Allee 11, 93042 Regensburg, Germany. sahar.abo-hamar@klinik.uni-regensburg.de
Objectives:
The purpose of this study was to evaluate the effect of either eugenol-containing or eugenol-free temporary cement removal by excavator or sandblasting on the shear bond strength of ceramic luted to dentin.
Methods:
A self-etching primer system, Panavia F 2.0, Kuraray Medical (PF2), and a total-etch bonding system, Excite/Variolink II, Vivadent (EXV), were used. One hundred and forty human molars, ground to expose dentin surfaces, were divided into 14 groups (seven groups for each adhesive system). For each adhesive system, either a eugenol-containing (Temp bond) or a eugenol-free (Temp bond NE) temporary cement was applied to the dentin surface for 7 days, then removed by an excavator or sandblasting (four groups). Three control groups were studied where fresh dentin was either scratched by excavator or sandblasted, or underwent no surface treatment. After application of the adhesives, ceramic cones (Cerafil inserts) were adhesively luted to standardized dentin areas. After 24 h storage in distilled water, the shear bond strengths were determined at a cross-head speed of 0.75 mm/min.
Results:
For each adhesive system, neither the method of temporary cement removal nor the type of temporary cement affected the bond strength significantly (P
Significance:
The use of temporary cements, either containing eugenol or not, does not alter the retentive strength of ceramic restorations luted to dentin using the tested adhesive systems, whether the temporary cements are removed by excavator or sandblasting.
Related Concept Videos
Bonding and Strength of Aggregate
Strength and Heat of Hydration
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...
Types of Cement I
Type I (Ordinary Portland Cement) is widely used for general construction where special properties are not required. It has moderate sulfate resistance and heat of hydration.
Type II (Modified Cement) offers moderate resistance to sulfate attack and a lower rate of heat development compared to Type I. It is suitable for structures in...
Soundness of Cement
Setting Time of Cement