Objectives:
The present study aims to evaluate the core-veneer bond strength and the cohesive strength of the components of three commercial layered all-ceramic systems. Two surface treatments for the core surface finish and different veneering ceramics with different thermal expansion coefficients (TEC) were applied. The selected systems were two CAD-CAM ceramics; Cercon and Vita Mark II and one pressable system; (IPS)Empress 2 for layering technique.
Methods:
Standardized core specimens were fabricated according to the manufacturer's instructions, or polished with 1200 siliconcarbide polishing paper. The core specimens were veneered with either its manufacturer's veneer or an experimental veneer with higher TEC. The obtained micro-bars were subjected to the microtensile bond strength test. The obtained data were analyzed using one and two-way ANOVA. A finite element analysis (FEA) model of the test setup was analyzed. Scanning Electron Microscopy (SEM) was carried out at the fracture surface.
Results:
The core materials were significantly stronger than the veneering materials and the layered core-veneer specimens of which the results were statistically comparable. Polishing the core surfaces did not have an effect on the core-veneer bond strength. Experimental veneer with higher TEC resulted in massive fractures in both the core and veneering material. SEM and FEA demonstrated fracture pattern and mechanism of failure.
Significance:
The core-veneer bond strength is one of the weakest links of layered all-ceramic restorations and has a significant role in their success. To exploit fully the high strength of zirconium oxide cores, further research work is needed to improve its bond with its corresponding veneering material.
Related Concept Videos
Bonding and Strength of Aggregate
Veneer
Other veneering techniques include plain-slicing, quarter-slicing, and rift-slicing. These...
Tensile Strength Considerations of Concrete
The dimensions and shape of a concrete specimen also...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...
Porosity in Cement Paste
The balance of water to cement in the mix is critical—it...
Tooth Anatomy
The Crown, Neck, and Root
The visible part of the tooth is referred to as the crown. It's covered by enamel, the hardest substance in the human body. The crown is uniquely shaped for each type of tooth, allowing for different functions such as cutting, tearing, or grinding food.