Related Experiment Video
Updated: Aug 14, 2026

Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
Influence of composite restorative materials and light-curing units on diametrical tensile strength
Maria Cecília Caldas Giorgi Tolosa1, Luís Alexandre Maffei Sartini Paulillo, Marcelo Giannini
1Department of Restorative Dentistry, School of Dentistry of Piracicaba, State University of Campinas.
Abstract:
The aim of this study was to evaluate the diametrical tensile strength (DTS) of three light-curing photo-activated composites with two different light curing units (LCU). Three types of dental restorative composites were used in this study: micro filled A110 (3M Espe); P60 (3M Espe) for posterior restorations, and micro-hybrid Charisma (Heraeus-Kulzer). The two LCUs were: halogen light (HAL) (Degulux, Degussa) and blue light emitting diode (LED) (Ultrablue, DMC). Resin composite specimens were inserted incrementally into a Teflon split mold measuring 3 mm in depth and 6 mm in internal diameter, and cured using either LCU (n = 10). Specimens were placed into a dark bottle containing distilled water at 37 degrees C for 7 days. DTS tests were performed in a Universal Testing Machine (0.5 mm/min). Data were submitted to two-way ANOVA and Tukey's test. Results were (MPa): A110/HAL: 276.50 +/- 62.94a; A110/LED: 306.01 +/- 65.16a; P60/HAL: 568.29 +/- 60.77b and P60/LED: 543.01 +/- 83.65b; Charisma/HAL: 430.94 +/- 67.28c; Charisma/LED: 435.52 +/- 105.12c. Results suggested that no significant difference in DTS was obtained with LCUs for the same composite. However, resin composite restorative materials presented different DTS.
Related Concept Videos
Relation Between Tensile Strength and Compressive Strength of Concrete
Tensile Strength Considerations of Concrete
The dimensions and shape of a concrete specimen also...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...