Resilient bioresorbable copolymers based on trimethylene carbonate, L-lactide, and 1,5-dioxepan-2-one
Natalia Andronova1, Ann-Christine Albertsson
1Department of Fibre and Polymer Technology, School of Chemistry Science and Engineering, Royal Institute of Technology, 100 44 Stockholm, Sweden.
Abstract:
The new combinations of monomers presented in this work were evaluated in order to create an elastic material for potential application in soft tissue engineering. Thermoplastic elastomers (TPE) of trimethylene carbonate (TMC) with L-lactide (LLA) and 1,5-dioxepan-2-one (DXO) have been synthesized using a cyclic five-membered tin alkoxide initiator. The block copolymers were designed in such a way that poly(trimethylene carbonate-co-1,5-dioxepan-2-one) formed an amorphous middle block and the poly(L-lactide) (PLLA) formed semicrystalline terminal blocks. The amorphous middle block consisted of relatively randomly distributed TMC and DXO monomer units, and the defined block structure of the PLLA terminal segments was confirmed by 13C NMR. The properties of the TMC-DXO-LLA copolymers were compared with those of triblock copolymers based either on LLA-TMC or on LLA-DXO. Differential scanning calorimetry and dynamic mechanical analysis data confirmed the micro-phase separation in the copolymers. The mechanical properties of the copolymers were evaluated using tensile testing and cycling loading. All of the copolymers synthesized showed a highly elastic behavior. The properties of copolymers could be tailored by altering the proportions of the different monomers.
Related Concept Videos
Bioplastics
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the polymer...