Related Experiment Video
Updated: Jul 19, 2026

Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
Evaluation of the fluoride release from orthodontic band cements
Senem Selvi Kuvvetli1, Elif Bahar Tuna, Sule Kavaloğlu Cildir
1Department of Pediatric Dentistry, Faculty of Dentistry, Yeditepe University, Istanbul, Turkey. sskuvvetli@yahoo.com.tr
Purpose:
To compare the fluoride levels released from a polyacid-modified resin composite (Ultra BandLok), a resin-modified glass-ionomer cement (Multicure) and a conventional glass-ionomer cement (Meron).
Methods:
Fluoride concentration in the deionized water was measured at 1, 2, 3, 7, 14 and 28 days. Fluoride measurement was undertaken using a fluoride ion selective electrode connected to an ion-analyzer. Friedman test was used in the repeated measurements of multiple groups. Kruskal-Wallis test was used to compare the groups. Dunn's multiple comparison test was applied for the comparison of subgroups.
Results:
The fluoride release pattern of the three materials was similar. The highest level of fluoride was obtained at the 24-hour measurement from all samples. According to comparisons among materials, Ultra BandLok released significantly less fluoride than Multicure and Meron (P < or = 0.01) at all the measurement times. In addition, the differences between the fluoride concentrations released from Multicure and Meron materials at all measurement days were not significant (P> 0.05).