Related Experiment Video
Updated: Jul 17, 2026

Electrospinning Fundamentals: Optimizing Solution and Apparatus Parameters
Published on: January 21, 2011
Preparation of CeO(2)-ZrO(2) ceramic fibers by electrospinning
Yanfei Zhang1, Jiayan Li, Qin Li
1Key Lab of Rare Earth Chemistry and Physics, Changchun Institute of Applied Chemistry, Chinese Academy of Sciences, Changchun 130022, Jilin, China.
Abstract:
Electrospinning was employed to fabricate polymer-ceramic composite fibers from solutions containing poly(vinyl pyrrolidone) (PVP), Ce(NO(3))(3) x 6H(2)O and ZrOCl(2) x 8H(2)O. Upon firing the composite fibers at 1000 degrees C, Ce(0.67)Zr(0.33)O(2) fibers with diameters ranging from 0.4 to 2 microm were synthesized. These fibers exhibit strong resistance to sintering. They still have specific surface area around 11.8 m(2)/g after being heated at 1000 degrees C for 6 h.