Atomic layer deposition on electrospun polymer fibers as a direct route to AL2O3 microtubes with precise wall

Qing Peng1, Xiao-Yu Sun, Joseph C Spagnola

  • 1Departments of Chemical and Biomolecular Engineering, North Carolina State University, Raleigh, North Carolina 27695, USA.

Nano Letters
|February 7, 2007