Microstructure of a newly developed gamma' strengthened Co-base superalloy

D H Ping1, C Y Cui, Y F Gu

  • 1High Temperature Materials Center, National Institute for Materials Science, Sengen 1-2-1, Tsukuba 305 0047, Japan. PING.De-hai@nims.go.jp

Ultramicroscopy
|March 27, 2007
PubMed

Related Concept Videos

Mechanical Characteristics of Steel01:18

Mechanical Characteristics of Steel

The mechanical characteristics of steel are assessed through various tests that evaluate its strength, toughness, and flexibility. These tests include tension, torsion, impact, bending, and hardness assessments, each providing crucial information about steel's suitability for specific applications.
The tension test is fundamental for determining tensile strength. In this test, a steel specimen is stretched using a gripping device until it breaks. The data collected during this test are used to...
Imperfections in Crystal Structure: Non-Stoichiometric Defects01:29

Imperfections in Crystal Structure: Non-Stoichiometric Defects

Non-stoichiometric defects refer to a type of defect in the crystal structure of a compound where the ratio of its constituent elements deviates from the ideal stoichiometric ratio. There are two main types of non-stoichiometric defects: metal excess defects and metal deficiency defects.Metal excess defects occur when there is a slight surplus of metal ions than what is required by the stoichiometric ratio of the compound. For example, heating a sodium chloride crystal in sodium vapor results...
Bonding and Strength of Aggregate01:12

Bonding and Strength of Aggregate

The bond between aggregate particles and the cement matrix is significantly influenced by the shape and surface texture of the aggregates. High-strength concretes benefit from a rougher texture, which leads to stronger bonding due to greater adhesion. Angular aggregates with larger surface areas also enhance this bond. The bonding quality, however, is complex to assess as no universally accepted test exists. Good bonding is indicated when a crushed concrete specimen shows some aggregate...