Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
Fracture resistance of short, randomly oriented, glass fiber-reinforced composite premolar crowns
Sufyan Garoushi1, Pekka K Vallittu, Lippo V J Lassila
1Department of Prosthetic Dentistry and Biomaterials Science, Institute of Dentistry, University of Turku, Lemminkäisenkatu 2, FI-20520 Turku, Finland. sufgar@utu.fi
Abstract:
The aim of this work was to determine the static load-bearing capacity of posterior composite crowns made of experimental composite resin (FC) with short fiber fillers and a semi-interpenetrating polymer network (IPN) matrix. In addition, we wanted to investigate how load-bearing capacity of surface composite resins was affected by substructures of fiber-reinforced composite (FRC) and FC, and by different curing systems. Five groups of crowns were fabricated (n=6). The crowns were either polymerized with a hand-light curing unit (LCU) or cured in a vacuum curing device (VLC) before they were statically loaded at a speed of 1mm min(-1) until fracture. Failure modes were visually examined. Data were analyzed using ANOVA. ANOVA revealed that crowns made from the FC had a statistically significant higher load-bearing capacity than the control PFC composite. Crowns with FRC substructure and PFC covering gave force values of 348N (LCU) and 1199N (VLC), respectively, which were lower than the values of FC composite. No statistically significant difference was found between crowns made from plain FC composite and those made from FC composite with a surface layer of PFC (P=0.892 and 1.00). Restorations made from short glass fiber-containing composite resin with IPN-polymer matrix showed better load bearing capacity than those made with either plain PFC or PFC reinforced with FRC substructure.
Related Concept Videos
Fiber Reinforced Concrete
Fractures: Bone Repair
Minor fractures with no bone displacement are treated by immobilizing the fractured bone using a cast or splint. However, in the case of fractures with displaced bones, the broken bones are repositioned before immobilization to ensure successful healing without deformation and loss of function. The realignment of fractured bone ends is performed through a process called reduction. If the procedure...
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...
Stress-Strain Diagram - Brittle Materials
Bonding and Strength of Aggregate
Toughness and Hardness of Aggregate