Atomic Force Microscopy Cantilever-Based Nanoindentation: Mechanical Property Measurements at the Nanoscale in Air and Fluid
Published on: December 2, 2022
Atomistic mechanisms and dynamics of adhesion, nanoindentation, and fracture
Abstract:
Molecular dynamics simulations and atomic force microscopy are used to investigate the atomistic mechanisms of adhesion, contact formation, nanoindentation, separation, and fracture that occur when a nickel tip interacts with a gold surface. The theoretically predicted and experimentally measured hysteresis in the force versus tip-to-sample distance relationship, found upon approach and subsequent separation of the tip from the sample, is related to inelastic deformation of the sample surface characterized by adhesion of gold atoms to the nickel tip and formation of a connective neck of atoms. At small tipsample distances, mechanical instability causes the tip and surface to jump-to-contact, which in turn leads to adhesion-induced wetting of the nickel tip by gold atoms. Subsequent indentation of the substrate results in the onset of plastic deformation of the gold surface. The atomic-scale mechanisms underlying the formation and elongation of a connective neck, which forms upon separation, consist of structural transformations involving elastic and yielding stages.
Related Concept Videos
Frictional Force
Tension Response at Adherens Junctions
α-Catenin as a Mechanosensory Protein
The α-catenin of adherens junctions is an allosteric protein with three VH (vinculin homology) domains...
Atomic Force Microscopy
The AFM Probe
The probe is regarded as the heart of any AFM setup and comprises the...
Dry Friction
To illustrate this concept, imagine a wooden crate resting on a rough, non-uniform horizontal surface. When an external force is applied to...