Scalable Step-by-Step Approach of Sustainable Bioplastic Production from Food Waste
Published on: July 18, 2025
Synthesis of polyhydroxyalkanoates in municipal wastewater treatment
Erik R Coats1, Frank J Loge, Michael P Wolcott
1Department of Civil Engineering, University of Idaho, Moscow, Idaho, USA.
Abstract:
Biologically derived polyesters known as polyhydroxyalkanoates (PHAs) represent a potentially "sustainable" replacement to fossil-fuel-based thermoplastics. However, current commercial practices that produce PHA with pure microbial cultures grown on renewable, but refined, feedstocks (i.e., glucose) under sterile conditions do not represent a sustainable commodity. Here, we report on PHA production with a mixed microbial consortium indigenous to an activated sludge process on carbon present in municipal wastewaters. Reactors operated under anaerobic/aerobic and aerobic-only mode and fed primary solids fermenter liquor maintained a mixed microbial consortium capable of synthesizing PHA at 10 to 25% (w/w), while reducing soluble COD by approximately 62 to 71%. More critically, an aerobic batch reactor seeded from the anaerobic/aerobic reactor and fed fermenter liquor achieved approximately 53% PHA (w/w). Results presented suggest that environmentally benign production of biodegradable polymers is feasible. We further used PHA-rich biomass to produce a natural fiber-reinforced thermoplastic composite that can be used to offset advanced wastewater treatment costs.
More Related Videos
Related Concept Videos
Bioplastics
Biological Treatment of Effluent and Waste Water
Microbial Bioremediation of Plastics
Production of Organic Acids
Microbial Wastewater Treatment
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the polymer...