Related Experiment Video
Updated: Jul 8, 2026

Use of Human Perivascular Stem Cells for Bone Regeneration
Published on: May 25, 2012
Minimum 10-year survival of Kerboull cemented stems according to surface finish
Moussa Hamadouche1, François Baqué, Nicolas Lefevre
1Clinical Orthopaedic Research Centre and the Department of Reconstructive and Orthopaedic Surgery, Université René Descartes (Paris 5), Hôpital Cochin (AP-HP), Paris, France. moussah@club-internet.fr
Unlabelled:
The optimal surface finish for a cemented THA stem is still debated. We hypothesized surface finish would influence survival of Kerboull cemented hip arthroplasties and a matte finish would have lower survival. We reviewed survival of 433 total hip arthroplasties in 395 patients: 284 consecutive patients (310 hips) were enrolled in a prospective, randomized study of polished (165 hips) or matte finish stems (145 hips) and compared to a historical series of satin stems (123 hips) in 111 patients. The satin and matte finish implants had similar geometry but the polished was quadrangular rather than oval. Finish roughnesses were: polished (radius, 0.04 microm), satin (radius, 0.9 microm), and matte (radius, 1.7 microm). The mean age of the patients at the time of the index arthroplasty was 63.6 years. The survival rate at 13 years, using radiographic loosening as the end point, was 97.3%+/-2.6% for polished stems, 97.1%+/-2.1% for satin stems, and 78.9%+/-5.8% for matte stems. The data suggest survival of Kerboull stems was higher with a polished or satin surface finish than with a matte finish.
Level Of Evidence:
Level II, therapeutic study. See the Guidelines for Authors for a complete description of levels of evidence.
Related Concept Videos
Types of Cement I
Type I (Ordinary Portland Cement) is widely used for general construction where special properties are not required. It has moderate sulfate resistance and heat of hydration.
Type II (Modified Cement) offers moderate resistance to sulfate attack and a lower rate of heat development compared to Type I. It is suitable for structures in...
Hydration of Cement
Curing of Concrete
Porosity in Cement Paste
The balance of water to cement in the mix is critical—it...
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...