Body distribution of poly(D,L-lactide-co-glycolide) copolymer degradation products in rats
1Shanghai Biomaterial Research and Test Center, Ninth People's Hospital, Shanghai Jiaotong University, No. 716, Xietu Road, Shanghai 200023, China.
Abstract:
Poly (D,L-lactide-co-glycolide) (PLGA) copolymers are among the few synthetic polymers approved for human use, but the biocompatibility of PLGA-derived oligomers and particles remains questionable. Here, high molecular weight PLGA (Mw=32,000) was radiolabeled with (125)I in chloroform solution, and the body distribution of PLGA copolymer degradation products was examined following subcutaneous implantation of round (125)I-PLGA films on the back of Sprague Dawley rats. Autoradiographic images of the PLGA implant taken at 2, 4, 6, 8, 10, and 12 weeks revealed that the central portion of the film degraded much more rapidly than the marginal portions. Examination of the body compartment distribution at these time points revealed that over one-half of the radioactivity was recovered from skin. The remaining radioactivity was concentrated in the blood, liver, and kidneys. Radioactivity steadily appeared in the blood and remained elevated up to 12 weeks after implantation, while the liver to kidney distribution began to decrease after 6 weeks. Cumulatively, these results indicate that the clearance of degraded particles and fragments from the implantation site is extremely delayed. Moreover, the degraded particles and fragments were selectively concentrated in the liver and kidneys, following release of degraded products into the bloodstream from the implantation site.
Related Concept Videos
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the polymer...
Microbial Bioremediation of Plastics
Polymers: Molecular Weight Distribution