Evaluation of biological stability and corrosion potential in drinking water distribution systems: a case study

C C Chien1, C M Kao, C W Chen

  • 1Institute of Environmental Engineering, National Sun Yat-Sen University, Kaohsiung, Taiwan.

Related Concept Videos

Quality of Water01:19

Quality of Water

In concrete preparation, the quality of water is paramount as it affects the strength and durability of the concrete. Potable water is usually preferred; however, it must not have excessive sodium or potassium to prevent compromising the concrete's integrity. Water quality is typically evaluated based on impurities such as dissolved solids, chlorides, and sulfates, and its pH value is ideally between 6 and 8. Even slightly acidic natural water may be acceptable unless it contains harmful...
Microbial Corrosion01:24

Microbial Corrosion

Microbiologically Influenced Corrosion (MIC) is a significant form of material degradation caused by the metabolic activities of microorganisms. This phenomenon poses substantial challenges across various industries, including oil and gas, maritime, and water treatment sectors.MIC occurs when microorganisms, such as bacteria, archaea, and fungi, colonize metal surfaces, forming biofilms that alter the local electrochemical environment. These biofilms can lead to the production of corrosive...
Testing Water Quality01:14

Testing Water Quality

When the quality of water for concrete preparation is uncertain, its impact on the setting time of cement and compressive strength of mortar is assessed by comparison with de-ionized or distilled water benchmarks. American Society for Testing and Materials (ASTM) C1602 requires the setting times to be within 90 minutes of the control, British Standard (BS) 3146:1980 allows a 30-minute variance in the initial setting, while British Standards European Norm (BS EN) 1008 specifies initial setting...
Corrosion of Reinforcement01:27

Corrosion of Reinforcement

The corrosion of steel reinforcement within concrete is a process influenced by the material's inherent properties and external factors. The high pH level of around 13, provided by calcium hydroxide present in concrete, initially protects the steel reinforcement by promoting the formation of a passive iron oxide layer on its surface.
However, over time and under certain conditions like carbonation, chloride ingress, and cracking this protective state can be compromised. Steel has areas with...
Precipitation and Co-precipitation01:17

Precipitation and Co-precipitation

Precipitation and coprecipitation methods can be used to separate a mixture of ions in a solution. In qualitative inorganic analysis, ions that form sparingly soluble precipitates with the same reagent are separated based on the differences in solubility products. For example, consider the separation of Cu(II) and Fe(II) ions by precipitation as insoluble sulfides. First, copper(II) sulfide is precipitated by the addition of acidic H2S, where the dissociation of H2S is suppressed. Adding H2S...
Waterproofing and Anti-Bacterial Admixtures in Concrete01:22

Waterproofing and Anti-Bacterial Admixtures in Concrete

Concrete's susceptibility to water absorption is due to the capillary action within the pores of its hydrated cement paste. This action draws water in, creating the need for waterproofing admixtures to prevent such penetration. The efficacy of these admixtures is contingent upon the water pressure, with variations arising from different conditions such as rain, capillary rise, or hydrostatic pressure in structures intended to hold water.
Waterproofing admixtures render concrete hydrophobic,...