Atomic layer deposition of metal oxides on pristine and functionalized graphene
Xinran Wang1, Scott M Tabakman, Hongjie Dai
1Department of Chemistry and Laboratory for Advanced Materials, Stanford University, Stanford, California 94305, USA.
Abstract:
We investigate atomic layer deposition (ALD) of metal oxide on pristine and functionalized graphene. On pristine graphene, ALD coating can only actively grow on edges and defect sites, where dangling bonds or surface groups react with ALD precursors. This affords a simple method to decorate and probe single defect sites in graphene planes. We used perylene tetracarboxylic acid (PTCA) to functionalize the graphene surface and selectively introduced densely packed surface groups on graphene. Uniform ultrathin ALD coating on PTCA graphene was achieved over a large area. The functionalization method could be used to integrate ultrathin high-kappa dielectrics in future graphene electronics.
More Related Videos
08:57Scalable Syntheses of Graphene Oxide and Reduced Graphene Oxide using Cascade Design Oxidation and Highly Basic Reduction Reactions
Published on: July 3, 2025
07:51Development and Functionalization of Electrolyte-Gated Graphene Field-Effect Transistor for Biomarker Detection
Published on: February 1, 2022