Related Experiment Video
Updated: Jul 3, 2026

Solvent Bonding for Fabrication of PMMA and COP Microfluidic Devices
Published on: January 17, 2017
Temperature rise and shear bond strength of bondable buccal tubes bonded by various light sources
Cagri Ulusoy1, Ozgür Irmak, Yildirim Hakan Bagis
1Department of Orthodontics, Gazi University, Ankara, Turkey. culusoy77@hotmail.com
Abstract:
The objective of the present investigation was to determine the intrapulpal temperature changes and to compare the shear bond strength (SBS) of bondable buccal tubes bonded by high-intensity light sources. Ninety caries-free human first molar teeth extracted for periodontal reasons were used. For the temperature measurement test, 30 teeth were randomly divided into three groups (n = 10) whereas 60 teeth were used in three groups (n = 20) for SBS testing. Three light sources, high-intensity halogen, blue light-emitting diode (LED), and xenon plasma arc (PAC), were used for polymerization of Transbond XT. Temperature variations (Delta T) were recorded by a K-type thermocouple wire connected to a data logger. For SBS testing, a universal testing machine was used at a crosshead speed of 1 mm/minute until buccal tube bonding failure occurred. Data were analyzed using the Kruskal-Wallis test. The high-intensity halogen light resulted in significantly (P < 0.01) higher intrapulpal temperature changes than the LED or PAC. The results of the shear bond test revealed significant (P < 0.05) differences only between the halogen and LED groups. The findings of the present investigation showed that high-intensity curing devices can safely be used in bonding buccal tubes to molar teeth without causing a deleterious effect on the dental pulp.
Related Concept Videos
Bonding and Strength of Aggregate
Bonding in Metals
Strength and Heat of Hydration
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...