Comparison of enamel and dentin microshear bond strengths of a two-step self-etching priming system with five
Michael F Burrow1, Yuichi Kitasako, C David Thomas
1School of Dental Science, The University of Melbourne, Victoria, Australia. mfburrow@unimelb.edu.au
Abstract:
Data on the adhesive strength of new all-in-one adhesives are still relatively limited. This study compared the microshear bond strengths of five recent all-in-one self-etching priming systems (G-Bond, One-Up Bond-F Plus, Clearfil S3 Bond, Adper Prompt L-Pop and Go!) with a widely used two-step self-etching priming system (Clearfil SE Bond). Human molars were sectioned and finished with 600-grit SiC paper. Both enamel and dentin were bonded using adhesives with a 0.7 mm bonding diameter. Bond strengths were tested using a microshear bond test method at a crosshead speed of 1 mm/minute. The mean bond strengths and standard deviations were calculated and analyzed using ANOVA and the Tukey's HSD test. Results showed the two-step self-etching system had significantly higher bond strengths to dentin. However, for enamel bond strength, Clearfil SE Bond showed no statistical difference to G-Bond and Go!; however, all of the other materials were statistically lower. It is necessary to examine these new materials clinically to determine their efficacy.