Polymeric materials based on main group elements: the recent development of ambient temperature and controlled routes
Vivienne Blackstone1, Alejandro Presa Soto, Ian Manners
1School of Chemistry, University of Bristol, Bristol, UKBS8 1TS.
Abstract:
This Perspective discusses the development of new routes to polyphosphazenes, [R(2)P[double bond, length as m-dash]N](n), that occur at ambient temperature and, in some cases, allow molecular weight control and access to narrow molecular weight distributions and block copolymers. For example, the room temperature silyl-carborane initiated ring-opening polymerisation of (NPCl(2))(3) is described together with chain growth condensation polymerisations of phosphoranimines Cl(3)P[double bond, length as m-dash]NSiMe(3) and BrMePhP[double bond, length as m-dash]NSiMe(3). Recent works on donor-stabilised cationic phosphoranimines are also discussed.
More Related Videos
12:07Fabricating Degradable Thermoresponsive Hydrogels on Multiple Length Scales via Reactive Extrusion, Microfluidics, Self-assembly, and Electrospinning
Published on: April 16, 2018
07:20Discovery and Synthesis Optimization of Isoreticular Al(III) Phosphonate-Based Metal-Organic Framework Compounds Using High-Throughput Methods
Published on: October 6, 2023
Related Concept Videos
Step-Growth Polymerization: Overview
Many natural and synthetic polymers are produced by...
Ziegler–Natta Chain-Growth Polymerization: Overview
Olefin Metathesis Polymerization: Ring-Opening Metathesis Polymerization (ROMP)
Polymers
Cationic Chain-Growth Polymerization: Mechanism
Types of Step-Growth Polymers: Polyesters
Polyesters are commonly prepared from terephthalic acid and ethylene glycol; the crude product is known as poly(ethylene terephthalate) or PET. However, polyesters are synthesized industrially by transesterification of dimethyl terephthalate with ethylene glycol at 150 °C. The two reactants and the polymer...