K-shell X-ray fluorescence measurements of arsenic depth-dependent concentration in polyester resin discs using the
Mihai R Gherase1, David E B Fleming
1Department of Physics, Mount Allison University, 67 York Street, Sackville, New Brunswick, Canada E4L 1E6.
Abstract:
In the realm of X-ray fluorescence (XRF) applications, inhomogeneous distribution of an element can occur as a function of depth within a sample. An example is the measurement of arsenic in skin; arsenic binds with non-uniformly distributed keratin. In this paper, an XRF signal equation based on the fundamental parameter (FP) method, which explicitly takes into account the depth dependence of the elemental concentration, was developed. The formalism was experimentally verified for two-disc resin stacks with different arsenic concentrations.
Related Concept Videos
Atomic Absorption Spectroscopy: Lab
Solutions containing organic solvents, such as low-molecular-mass alcohols, esters, or ketones, enhance absorbances by increasing nebulizer...
Atomic Fluorescence Spectroscopy
Atomic Emission Spectroscopy: Lab
Atomic Absorption Spectroscopy: Overview
When irradiated by EMR of a particular wavelength, these...
Atomic Emission Spectroscopy: Overview
Atomic Emission Spectroscopy: Instrumentation