Sand/cement ratio evaluation on mortar using neural networks and ultrasonic transmission inspection

M Molero1, I Segura, M A G Izquierdo

  • 1Departamento de Señales, Sistemas y Radiocomunicaciones, ETSI Telecomunicación (UPM), Spain. molero@iai.csic.es

Ultrasonics
|October 9, 2008
PubMed

Related Concept Videos

Strength of Cement01:20

Strength of Cement

Strength tests for cement are not performed directly on neat cement paste due to difficulty in obtaining consistent, reliable specimens. Instead, cement is typically tested in the form of cement-sand mortar.
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...
Fineness of Cement01:15

Fineness of Cement

The fineness of cement directly influences the rate of hydration, as the hydration begins at the surface of the cement particles. In addition to hydration, the fineness of cement is vital for various properties of concrete including workability, gypsum requirement, and long-term behavior. The fineness of cement is represented in terms of the specific surface of cement which is typically measured in square meters per kilogram, with several methods available for this determination.
Direct...
Aggregate Cement Ratio01:21

Aggregate Cement Ratio

The Aggregate Cement ratio refers to the weight of aggregate divided by the weight of cement in a concrete mix. Altering this ratio has profound effects on the concrete's properties. This ratio plays a pivotal role in determining the strength, workability, and durability of concrete. When the Aggregate Cement ratio is higher, the mix is leaner, meaning it has less cement paste to lubricate the aggregate, potentially making the concrete less workable. Such mixes, known as lean, enhance the...
Microcracking in Concrete01:20

Microcracking in Concrete

Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
Mortar Joint Deterioration in Masonry01:13

Mortar Joint Deterioration in Masonry

Mortar joint deterioration is a significant concern in masonry structures, with water accumulation in the joints leading to damage from freeze-thaw cycles. The repeated expansion of water during freezing and its melting during thawing develop and propagate cracks in the masonry joints. Eventually, this leads to the spalling of mortar from the joints, loosening masonry units and weakening the structure. The deteriorated mortar joints are also vulnerable to moisture intrusion into the walls.
The...
Water Cement Ratio01:28

Water Cement Ratio

The water-cement ratio is pivotal in defining concrete's quality. This ratio, a balance between the weight of water and cement in the mix, shapes the concrete's strength, durability, and resistance to environmental factors. As identified by Abrams’ law, less water in the mix equates to stronger concrete. However, water is essential not only for the chemical process of hydration but also for the concrete's workability and compaction. While hydration chemically binds water and cement, physical...