Influence of water storage time on the bond strength of etch-and-rinse and self-etching adhesive systems

Darlene Cristina Ramos Eloy Dantas1, Ana Isabella Arruda Meira Ribeiro, Lúcia Helena Marques de Almeida Lima

  • 1Department of Dentistry, State University of Paraíba, Campina Grande, PB, Brazil.

Brazilian Dental Journal
|October 25, 2008
PubMed

Related Concept Videos

Testing Water Quality01:14

Testing Water Quality

When the quality of water for concrete preparation is uncertain, its impact on the setting time of cement and compressive strength of mortar is assessed by comparison with de-ionized or distilled water benchmarks. American Society for Testing and Materials (ASTM) C1602 requires the setting times to be within 90 minutes of the control, British Standard (BS) 3146:1980 allows a 30-minute variance in the initial setting, while British Standards European Norm (BS EN) 1008 specifies initial setting...
Effect of Sea Water on Concrete01:22

Effect of Sea Water on Concrete

Concrete exposed to seawater can undergo degradation like the dissolution of ettringite and gypsum, increasing the material's porosity and decreasing its strength. In contrast, the crystallization of salts within the concrete's pores can cause expansion, particularly above the waterline where evaporation occurs. Nonetheless, this expansion only happens when seawater, enabled by the concrete's permeability, manages to infiltrate the structure.
Concrete in areas between tide marks, which undergo...
Strength and Heat of Hydration01:29

Strength and Heat of Hydration

The hydration of cement is an exothermic reaction in which heat is generated as cement hydrates. This heat of hydration is critical to cement's strength development. The rate at which this heat is generated affects the temperature rise, with a majority of the heat being released early in the hydration process, half within the first three days, and about 75% within the first week.
The heat of hydration for each cement compound is significant; for instance, tricalcium aluminate (C3A) and...
Bonding and Strength of Aggregate01:12

Bonding and Strength of Aggregate

The bond between aggregate particles and the cement matrix is significantly influenced by the shape and surface texture of the aggregates. High-strength concretes benefit from a rougher texture, which leads to stronger bonding due to greater adhesion. Angular aggregates with larger surface areas also enhance this bond. The bonding quality, however, is complex to assess as no universally accepted test exists. Good bonding is indicated when a crushed concrete specimen shows some aggregate...
Waterproofing and Anti-Bacterial Admixtures in Concrete01:22

Waterproofing and Anti-Bacterial Admixtures in Concrete

Concrete's susceptibility to water absorption is due to the capillary action within the pores of its hydrated cement paste. This action draws water in, creating the need for waterproofing admixtures to prevent such penetration. The efficacy of these admixtures is contingent upon the water pressure, with variations arising from different conditions such as rain, capillary rise, or hydrostatic pressure in structures intended to hold water.
Waterproofing admixtures render concrete hydrophobic,...
Curing of Concrete01:20

Curing of Concrete

The hydration of cement takes place within the water-filled capillary pores. However, environmental elements can disrupt this process by evaporating water from the concrete surfaces. Sealed concrete with a water-cement ratio below 0.5 experiences self-desiccation, leading to water loss. The water loss in concrete is mitigated by curing. This technique involves keeping the concrete saturated to maintain the necessary temperature and moisture conditions, to optimally fill the spaces in the cement...