Indirect measurement of the magnetocaloric effect using a novel differential scanning calorimeter with magnetic field

S Jeppesen1, S Linderoth, N Pryds

  • 1Fuel Cells and Solid State Chemistry Department, Riso DTU, Technical University of Denmark, DK-4000 Roskilde, Denmark.

Related Concept Videos

Constant Pressure Calorimetry03:02

Constant Pressure Calorimetry

Calorimetry is a technique used to measure the amount of heat involved in a chemical or physical process or to measure the heat transferred to or from a substance. The heat is exchanged with a calibrated and insulated device called the calorimeter. Calorimetry experiments are based on the assumption that there is no heat exchange between the insulated calorimeter and the external environment. The well-insulated calorimeters prevent the transfer of heat between the calorimeter and its external...
Diamagnetism01:26

Diamagnetism

Materials consisting of paired electrons have zero net magnetic moments. However, when these materials are placed under an external magnetic field, the moments opposite to the field are induced. Such materials are called diamagnets. Diamagnetism is the response of the diamagnets when placed in an external magnetic field.
Diamagnetism was discovered by Anton Brugmans in 1778 when he observed that bismuth gets repelled by magnetic fields, thus theorizing that diamagnets get repelled by magnets.
Magnetic Susceptibility and Permeability01:31

Magnetic Susceptibility and Permeability

In linear magnetic materials, like paramagnets and diamagnets, magnetization is proportional to the magnetic field intensity. The constant of proportionality, a dimensionless number, is called magnetic susceptibility. The value of the susceptibility depends on the type of material.
When diamagnetic materials are placed under an external magnetic field, the moments opposite to the field are induced. Hence, the susceptibility for diamagnets has a minimal negative value of 10-5–10-6. Since...
Ferromagnetism01:31

Ferromagnetism

Materials like iron, nickel, and cobalt consist of magnetic domains, within which the magnetic dipoles are arranged parallel to each other. The magnetic dipoles are rigidly aligned in the same direction within a domain by quantum mechanical coupling among the atoms. This coupling is so strong that even thermal agitation at room temperature cannot break it. The result is that each domain has a net dipole moment. However, some materials have weaker coupling, and are ferromagnetic at lower...
Calorimetry01:19

Calorimetry

When objects at different temperatures are placed in contact with each other but isolated from everything else, they attain thermal equilibrium. A container that prevents heat transfer in or out is called a calorimeter, and the use of a calorimeter to make measurements is called calorimetry. Generally, these measurements involve heat or specific heat capacity. The term "calorimetry problem" is used for any problem where the specified objects are thermally isolated from their surroundings. An...
Paramagnetism01:30

Paramagnetism

Paramagnets are materials with unpaired electrons that possess a finite magnetic moment. In the absence of a magnetic field, these moments are randomly oriented, and thus the net moment is zero. Under an external field, a torque acting on the moments tends to align them along the field's direction. However, the random thermal motion of electrons produces a torque opposite to the external field and tries to disorient the moments. These two competing effects align only a few moments along the...