Nanoindentation of gold nanoparticles functionalized with proteins

Heeyeon P Wampler1, Albena Ivanisevic

  • 1Department of Chemistry, Purdue University, West Lafayette, IN 47907, United States.

Micron (Oxford, England : 1993)
|March 17, 2009
PubMed