Density functional theory, molecular dynamics, and differential scanning calorimetry study of the RbF-CsF phase

O Benes1, Ph Zeller, M Salanne

  • 1European Commission, Joint Research Centre, Institute for Transuranium Elements (ITU), P.O. Box 2340, 76125 Karlsruhe, Germany. ondrej.benes@cea.fr