Related Experiment Video
Updated: Jun 22, 2026

Quasistatic Mechanical Testing for Computer-Aided Design and Manufacturing Occlusal Veneers Cemented to Milled Dentin Analog Material
Published on: December 20, 2024
Flexural strength and hardness of direct and indirect composites
Márcia Borba1, Alvaro Della Bona, Dileta Cecchetti
1Dental Materials, University of São Paulo, SP, Brazil.
Abstract:
The objective of this study was to evaluate the flexural strength (sigma f) and hardness (H) of direct and indirect composites, testing the hypotheses that direct resin composites produce higher sigma f and H values than indirect composites and that these properties are positively related. Ten bar-shaped specimens (25 mm x 2 mm x 2 mm) were fabricated for each direct [D250 - Filtek Z250 (3M-Espe) and D350 - Filtek Z350 (3M-Espe)] and indirect [ISin - Sinfony (3M-Espe) and IVM - VitaVM LC (Vita Zahnfabrik)] materials, according to the manufacturer's instructions and ISO4049 specifications. The sigma f was tested in three-point bending using a universal testing machine (EMIC DL 2000) at a crosshead speed of 0.5 mm/min (ISO4049). Knoop hardness (H) was measured on the specimens' fragments resultant from the sigma f test and calculated as H = 14.2P/l(2), where P is the applied load (0.1 kg; dwell time = 15 s) and l is the longest diagonal of the diamond shaped indent (ASTM E384). The data were statistically analyzed using Anova and Tukey tests (alpha = 0.05). The mean sigma f and standard deviation values (MPa) and statistical grouping were: D250 - 135.4 +/- 17.6a; D350 - 123.7 +/- 11.1b; ISin - 98.4 +/- 6.4c; IVM - 73.1 +/- 4.9 d. The mean H and standard deviation values (kg/mm(2)) and statistical grouping were: D250 - 98.12 +/- 1.8a; D350 - 86.5 +/- 1.9b; ISin - 28.3 +/- 0.9 c; IVM - 30.8 +/- 1.0 c. The direct composite systems examined produce higher mean sigma f and H values than the indirect composites, and the mean values of these properties were positively correlated (r = 0.91), confirming the study hypotheses.
Related Concept Videos
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...
Flexural Stress
Hooke's Law states that within the material's elastic limits, stress is directly proportional to strain. In a member experiencing a bending moment, the strain at any point is relative to its distance...
Bending of Members Made of Several Materials
Hooke's Law determines stress in each material, stating that stress is proportional to strain but varies due to each material's...
Relation Between Tensile Strength and Compressive Strength of Concrete
Tensile Strength Considerations of Concrete
The dimensions and shape of a concrete specimen also...
Fiber Reinforced Concrete