Inspection of deteriorating asbestos cement force mains with georadar technique

S Smolders1, L Verhoest, G De Gueldre

  • 1Research and Product Development Division, Aquafin N.V., Dijkstraat 8, 2630, Aartselaar, Belgium. sven.smolders@aquafin.be

Related Concept Videos

Non-destructive Tests for Concrete Strength01:12

Non-destructive Tests for Concrete Strength

The rebound hammer test, also known as the Schmidt hammer test, is a non-destructive technique for evaluating the hardness of concrete and, indirectly, the strength of concrete. It operates on the principle that the rebound of a spring-driven mass from a concrete surface correlates to the surface's hardness. The device comprises a mass within a tubular housing, a spring mechanism, and a plunger that strikes the concrete. Upon release, the energy imparted to the mass by the spring causes it to...
Mortar Joint Deterioration in Masonry01:13

Mortar Joint Deterioration in Masonry

Mortar joint deterioration is a significant concern in masonry structures, with water accumulation in the joints leading to damage from freeze-thaw cycles. The repeated expansion of water during freezing and its melting during thawing develop and propagate cracks in the masonry joints. Eventually, this leads to the spalling of mortar from the joints, loosening masonry units and weakening the structure. The deteriorated mortar joints are also vulnerable to moisture intrusion into the walls.
The...
Microcracking in Concrete01:20

Microcracking in Concrete

Microcracking in concrete refers to the tiny cracks that can form within the material even before any external load is applied. These microcracks typically occur at the interface between the coarse aggregate and the hydrated cement paste, often as a result of differential volume changes prompted by variations in stress-strain behavior, as well as thermal and moisture movement. Initially, these microcracks remain stable and do not grow substantially until the concrete is stressed to about 30...
Testing Water Quality01:14

Testing Water Quality

When the quality of water for concrete preparation is uncertain, its impact on the setting time of cement and compressive strength of mortar is assessed by comparison with de-ionized or distilled water benchmarks. American Society for Testing and Materials (ASTM) C1602 requires the setting times to be within 90 minutes of the control, British Standard (BS) 3146:1980 allows a 30-minute variance in the initial setting, while British Standards European Norm (BS EN) 1008 specifies initial setting...
Fiber Reinforced Concrete01:22

Fiber Reinforced Concrete

Fiber-reinforced concrete significantly enhances the structural and nonstructural properties of traditional concrete by incorporating fibers like steel, glass, and polymers. These fibers, varying from natural ones such as sisal and cellulose to manufactured ones like polypropylene and Kevlar, are mixed into hydraulic cement with aggregates. Steel fibers, often preferred for their robustness, contribute to improved ductility, toughness, and post-cracking performance. The concrete is classified...
Deleterious Substances in Aggregate01:25

Deleterious Substances in Aggregate

Deleterious substances in aggregates can be detrimental to the quality and durability of concrete. These substances include organic impurities like loam, which interfere with cement hydration and are usually present in the sand. These prevent a good bond between aggregate and cement paste. Organic impurities can be detected using the colorimetric test, where the darkness of a solution after agitation indicates the level of organic content.
Another type of impurity is clay and fine material that...