Contribution of Ni KLL Auger electrons to the probing depth of the conversion electron yield measurements
Related Experiment Video
Updated: Jun 16, 2026

All-electronic Nanosecond-resolved Scanning Tunneling Microscopy: Facilitating the Investigation of Single Dopant Charge Dynamics
Published on: January 19, 2018
Shinjiro Hayakawa1, Aya Tanaka, Takeshi Hirokawa
1Department of Applied Chemistry, Graduate School of Engineering, Hiroshima University, Japan. hayakawa@hiroshima-u.ac.jp
Abstract:
The averaged attenuation length of emitted electrons with the conversion electron yield (CEY) method was evaluated for Ni films with the x-rays below and above the Ni K absorption edge. The evaluated attenuation length was 13.1 nm with the x-rays below the Ni K absorption edge, and it became 24.0 nm with the contribution of Ni KLL Auger electrons that had the attenuation length of 78.1 nm. The probing depth of the CEY measurements are determined both the penetration depth of x-rays and the attenuation length of emitted electrons, and the modification of the probing depth was investigated with the grazing incidence condition. The glancing angle dependence of the CEY was compared with the model calculation, and the probing depth of around 1.6 nm was realized under the total reflection condition. The probing depth was controlled from 1.6 nm to the attenuation length by changing the glancing angle.
More Related Videos
14:11Quantification of Hydrogen Concentrations in Surface and Interface Layers and Bulk Materials through Depth Profiling with Nuclear Reaction Analysis
Published on: March 29, 2016
14:53In Situ Detection and Single Cell Quantification of Metal Oxide Nanoparticles Using Nuclear Microprobe Analysis
Published on: February 3, 2018
Related Concept Videos
Nuclear Overhauser Enhancement (NOE)
Scanning Electron Microscopy
Fundamental Principles
Accelerated...
¹³C NMR: Distortionless Enhancement by Polarization Transfer (DEPT)
Overview of Microscopy Techniques