Evaluating anisotropic properties in the porcine temporomandibular joint disc using nanoindentation
Related Experiment Video
Updated: Jun 15, 2026

Addressing Practical Issues in Atomic Force Microscopy-Based Micro-Indentation on Human Articular Cartilage Explants
Published on: October 28, 2022
P A Yuya1, E K Amborn, M W Beatty
1Department of Engineering Mechanics, University of Nebraska-Lincoln, Lincoln, NE 68588-0526, USA.
Abstract:
The objective of this study was to determine the viscoelastic properties present within the intermediate zone of the porcine temporomandibular joint (TMJ) disc using nanoindentation. A 50-microm conospherical indenter tip using a displacement-controlled ramp function with a 600 nm/s loading and unloading rate, a 3000-nm peak displacement with a holding period of 30 s was used to indent the samples. Experimental load-relaxation tests were performed on the TMJ disc to determine the response in three different directions; the mediolateral, anteroposterior, and articular surface directions. The experimental data were analyzed using a generalized Maxwell model to obtain values for short- and long-time relaxation modulus and of material time constants. The short time relaxation modulus E ( I ) values were 180.92, 64.99, and 487.77 kPa for testing done on the articular surface, mediolateral, and anteroposterior directions, respectively. Corresponding values for the long-time relaxation modulus E (infinity) were 45.9, 14.97, and 133.5 kPa. The method confirmed anisotropy present within the central intermediate zone of the porcine TMJ disc due to the directional orientation of the collagen fibers.