Related Experiment Video
Updated: Jun 14, 2026

Methods for Facilitating Microbial Growth on Pulp Mill Waste Streams and Characterization of the Biodegradation Potential of Cultured Microbes
Published on: December 12, 2013
The pyrolytic degradation of wood-derived lignin from pulping process
1Energy Technology Research Group, School of Engineering Science, University of Southampton, Highfield, Southampton SO17 1BJ, United Kingdom.
Abstract:
Lignin is a key component in the biomass with a complex polymeric structure of the phenyl-C(3) alkyl units. The kraft lignin from the wood pulping process is tested in TG-FTIR and Py-GC-MS. The samples are pyrolyzed in TGA coupled with FTIR from 30 to 900 degrees C at the heating rate of 20 and 40K/min. The evolution of phenolic compounds in the initial pyrolysis stage of lignin is determined by FTIR, while the second stage is mainly attributed to the production of the low molecular weight species. A bench-scale fast pyrolysis unit is employed to investigate the effect of temperature on the product yield and composition. It is found that the guaiacol-type and syringol-type compounds as the primary products of lignin pyrolysis are predominant in bio-oil, acting as the significant precursors for the formation of the derivatives such as the phenol-, cresol- and catechol-types. A series of free-radical chain-reactions, concerning the cracking of different side-chain structures and the methoxy groups on aromatic ring, are proposed to demonstrate the formation pathways for the typical compounds in bio-oil by closely relating lignin structure to the pyrolytic mechanisms. The methoxy group (-OCH(3)) is suggested to work as an important source for the formation of the small volatile species (CO, CO(2) and CH(4)) through the relevant free radical coupling reactions.
Related Concept Videos
Wood Products
Glue-laminated wood, often referred to as glulam, combines multiple smaller pieces of dimensional lumber using adhesives to form a single, larger piece. Cross-laminated timber consists...
Biodeterioration
Lumber
Initially, the surfaces of these lumber pieces are rough, and their dimensions may vary slightly from one end to...
Introduction to Wood
The structural integrity of the wood...
Lumber Defects