[Bond durability of self-adhesive resin cement to glass ceramic]
Xiang-Feng Meng1, Qing Liu, Xiao-Ping Luo
1Department of Prosthodontics, School of Stomatology, Nanjing University & Nanjing Stomatological Hospital, Nanjing 210008, China. mengsoar@nju.edu.cn
Objective:
To evaluate the bond durability of glass ceramic to self-adhesive and conventional resin cements.
Methods:
Maximum water sorption and solubility of two resin cements (A: self-adhesive type, G-CEM; B: conventional type, Linkmax HV) were measured during 6 week water storage. And their surface Knoop hardness number was measured at 0.5, 24 h and 6 week after irradiation. Sixty-four glass ceramic samples were or were not silanized with one of the three silane coupling agents (A: Monobond S; B: Clearfil Ceramic Primer; C: GC Ceramic Primer), and then cemented with two resin cements. The micro-bond strength between the two cements and glass ceramic were measured at baseline and after 30 000 thermal cycle.
Results:
Cement A had higher water sorption [(79.62 +/- 5.63) microg/mm³] and solubility [(4.78 +/- 3.33) microg/mm³] than cement B[(35.03 +/- 3.33) microg/mm³, (0.00 +/- 0.00) microg/mm³]. Cement A and B could achieve maximal surface hardness at 24 h after irradiation, and this was maintained during 6 week water storage. After 30 000 thermal cycle, the micro-bond strength between unsilanized glass ceramic and cement A or B was (0.00 +/- 0.00) MPa, and those between cement A and silanized glass ceramic with silane coupling agent A, B and C, were (2.86 +/- 3.25), (12.75 +/- 1.55) and (11.98 +/- 2.35) MPa respectively [for cement B, the data was (5.15 +/- 5.20), (10.94 +/- 3.30) and (14.18 +/- 3.13) MPa]. No significant diffrence was found between the micro-bond strength of cement A and that of cement B with glass ceramic.
Conclusions:
Self-adhesive resin cement can achieve similar bond durability to glass ceramic as conventional resin cement does.
Related Concept Videos
Bonding and Strength of Aggregate
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...
Mortar Properties
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...
Aggregate Cement Ratio
Types of Cement II