Evaluating the Effects of Different Polishing Methods on Color Stability of Dental Restorations in Pediatric Dentistry
Published on: June 6, 2025
Colour stability of veneering composites after accelerated aging
Triantafillos Papadopoulos1, Aspasia Sarafianou, Andreas Hatzikyriakos
1Associate Professor, Department of Biomaterials, School of Dentistry, National and Kapodistrian University of Athens, Athens, Greece.
Objectives:
To investigate the colour stability of four indirect composite restorative materials after accelerated aging.
Methods:
Four indirect composites (Gradia, Signum+, HFO and Adoro) were used. For each material, six specimens were prepared and subjected to accelerated aging (Suntest CPS+, Atlas, Chicago, IL, USA) according to ISO 7491. A Dr. Lange Microcolor Data Station colorimeter (Braive Instruments, Liege, Belgium) was used to measure specimen colour before and after aging. Measurements were performed according to the CIE L*a*b* system, and the mean L*, a* and b* values for each material were calculated. The equation DeltaE = [(DeltaL*)2 + (Deltaa*)2 + (Deltab*)2](1/2) was used to measure the total colour change (DeltaE), where DeltaL*, Deltaa* and Deltab* are the differences in the respective values before and after aging. One-way ANOVA were used to determine statistically significant differences in DeltaL*, Deltaa*, Deltab* and DeltaE.
Results:
No statistically significant differences were found in DeltaL*, Deltaa*, Deltab* and DeltaE among the materials tested (PDeltaL*=.063; PDeltaa*=.521; PDeltab*=.984 and PDeltaE=.408). After aging, Gradia specimens showed an increase in lightness (DeltaL*=0.36) and a green-yellow shift (Deltaa*=-1.18, Deltab*=0.6), while Signum+ specimens exhibited an increase in lightness (DeltaL*=0.5) and a green-blue shift (Deltaa*=-0.9, Deltab*=-0.45). HFO specimens exhibited an increase in lightness (DeltaL*=0.75) and a green-yellow shift (Deltaa*=-1.3, Deltab*=0.06), and Adoro specimens exhibited an increase in lightness (DeltaL*=2.07) and a green-yellow shift (Deltaa*=-1.3, Deltab*=0.68).
Conclusions:
Colour changes were found to be within accepted values of perceptibility and clinical acceptance after accelerated aging, and no statistically significant differences were found in DeltaL*, Deltaa*, Deltab* and DeltaE among the materials tested.
Related Concept Videos
Veneer
Other veneering techniques include plain-slicing, quarter-slicing, and rift-slicing. These...
Accelerated Curing of Concrete
Drug Product Stability
The Effect of Aging on Tissues
Abrasion Resistance of Concrete
One such test is the revolving disc test, where three plates...
Effects of EDTA on End-Point Detection Methods
In the visual method, metal-ion indicators (metallochromic dyes), which have distinct colors in their free and complex forms, are added to the mixture to signal the titration's end point. They form stable complexes with metal ions, but these complexes are weaker than the corresponding metal–EDTA complexes. As a result, EDTA...