Related Experiment Video
Updated: Jun 10, 2026

Scanning Electron Microscopic Evaluation of Surface Defects of Remover Retreatment File After Single and Multiple Uses
Published on: October 11, 2024
Effects of raw material and rotational speed on the cyclic fatigue of ProFile Vortex rotary instruments
Yong Gao1, Vincent Shotton, Kevin Wilkinson
1DENTSPLY Tulsa Dental Specialties, Tulsa, OK 74135, USA. yong.gao@dentsply.com
Introduction:
This in vitro study compared the cyclic fatigue resistance of ProFile Vortex rotary instruments (DENTSPLY Tulsa Dental, Tulsa, OK) made of two different raw materials: M-Wire and regular superelastic wire (SE-wire) at two different rotational speeds. Two rotary-based Profile Vortex instruments with taper 0.04 and 0.06 (25 mm in length and #30 in size) were compared.
Methods:
Cyclic fatigue testing was performed by rotating instruments in an artificially constructed stainless steel canal with a 5-mm radius and a 90 degrees angle of curvature at two different test frequencies: 300 and 500 rpm. The time to failure was recorded, and the total number of cycles to failure was calculated and compared for a total of 160 samples. Statistical analysis was performed with one-way analysis of variance and the Tukey test for individual comparisons (confidence level of p < 0.05). Fracture surfaces of broken instruments were also observed under scanning electron microscopy. Over 50% of broken files made of SE-wire exhibited multiple crack initiation sites compared with the single crack initiation on files made of M-Wire.
Results:
Overall, there were significant differences in rotary instruments made of different materials (p < 0.001). However, for rotary instruments made from the same material (either M-Wire or SE-wire), there was no significant difference (p > 0.05) of cyclic fatigue life under different rotational speeds (300 and 500 rpm).
Conclusions:
ProFile Vortex files made of M-Wire exhibited superior cyclic fatigue resistance (approximately 150% longer in fatigue life) compared with those made of regular SE-wire at two test frequencies (300 and 500 rpm).
Related Concept Videos
Fatigue
Residual Stresses in Circular Shafts
Plastic Deformation in Circular Shafts
Stress Concentrations in Circular Shafts
Transmission Shafts: Problem Solving
Next, use bending moment diagrams for the shaft to...
Thin-Walled Hollow Shafts