Objective:
To analyze the reliability of all-ceramic crown on mandibular first molar under randomized biting force, and to explore the failure possibility of all-ceramic crown.
Methods:
Finite element (FE) models of all-ceramic crown on mandibular first molar were established using the Algor FE software. All-ceramic crown was loaded at different occlusal areas and positions with random variables of biting force, and the reliability of all-ceramic crown was analyzed.
Results:
The occlusal contact positions were located on the fossa, inclined surface and dental cusp. When the occlusal contact area was 0.4 mm(2), The reliability of all-ceramic crown on mandibular first molar were 100% (fossa), 99% (inclined surface), and 97% (cusp) respectively. When the occlusal contact area was 1.5 mm(2), the reliabilities of all-ceramic crown on mandibular first molar were 100% (fossa), 100% (inclined surface), and 99% (cusp) respectively. When the occlusal contact area was increased to 12.6 mm(2), the reliability of all-ceramic crown was 100%.
Conclusions:
Premature occlusal contact and steep cusp inclination on all-ceramic crown on mandibular first molar will result in stress concentration and the crown will exhibit high failure probabilities. Chewing hard food is another contributing factor to the failure of all-ceramic crowns.