Simulation of cemented granular materials. II. Micromechanical description and strength mobilization at the onset of
Nicolas Estrada1, Arcesio Lizcano, Alfredo Taboada
1Departamento de Ingeniería Civil y Ambiental-CeiBA Complex Systems Research Center, Universidad de Los Andes, Bogotá, Colombia. n.estrada22@uniandes.edu.co
Abstract:
This is the second of two papers investigating the mechanical response of cemented granular materials by means of contact dynamics simulations. In this paper, a two-dimensional polydisperse sample with high void ratio is sheared in a load-controlled simple shear numerical device until the stress state of the sample reaches the yield stress. We first study the stress transmission properties of the granular material in terms of the fabric of different subsets of contacts characterized by the magnitude of their normal forces. This analysis highlights the existence of a peculiar force carrying structure in the cemented material, which is reminiscent of the bimodal stress transmission reported for cohesionless granular media. Then, the evolution of contact forces and torques is investigated trying to identify the micromechanical conditions that trigger macroscopic yielding. It is shown that global failure can be associated to the apparition of a group of particles whose contacts fulfill at least one of the local rupture conditions. In particular, these particles form a large region that percolates through the sample at the moment of failure, evidencing the relationship between macroscopic yielding and the emergence of large-scale correlations in the system.
More Related Videos
06:54A Virtual Simulation Experiment of Mechanics: Material Deformation and Failure Based on Scanning Electron Microscopy
Published on: January 20, 2023
11:38Environmentally-controlled Microtensile Testing of Mechanically-adaptive Polymer Nanocomposites for ex vivo Characterization
Published on: August 20, 2013
Related Concept Videos
Microcracking in Concrete
Plastic Behavior
Strength of Cement
For compressive strength tests, ASTM C 109-05 standards prescribe a cement-sand mix ratio of 1:2.75 and a water/cement ratio of 0.485 for making 2-inch cubes. These cubes are mixed, cast, and cured in saturated lime water at 23°C until testing. Flexural strength testing, outlined in ASTM C...
Tensile Strength Considerations of Concrete
The dimensions and shape of a concrete specimen also...
Yield Criteria for Ductile Materials under Plane Stress
The Maximum Shearing Stress Criterion, also known as the...
Stress-Strain Diagram - Brittle Materials