Abstract:
Potassium oxalate desensitizers were previously shown to effectively reduce the immediate permeability of resin-bonded dentin. The current study evaluated whether the effect of the combined application of oxalate with etch-and-rinse adhesives interferes with the durability of resin-dentin bonds when using etch-and-rinse adhesives. The bond strength of resin-bonded dentin specimens composed of two-step or three-step etch-and-rinse adhesives (Single Bond, One-Step and Scotchbond Multi-Purpose, respectively) was tested immediately (24 hours) and after 12 months of water storage. The adhesives were used either according to the manufacturers' instructions (control groups) or after treating acid-etched dentin with a potassium oxalate gel (BisBlock, BISCO, Inc). The treatment of dentin with potassium oxalate was shown to negatively affect the baseline bond strength of resin-bonded dentin specimens, regardless of the adhesive used (p < 0.05). After storage, the bond strength of the resin-bonded interfaces was significantly reduced for all the tested groups (p < 0.001). Nevertheless, the rate of decreasing bond strength was significantly lower for oxalate-treated specimens than for the controls (p < 0.05).