Atomic layer deposition of titanium dioxide on cellulose acetate for enhanced hemostasis
Related Experiment Video
Updated: Jun 4, 2026

Photopatterning Proteins and Cells in Aqueous Environment Using TiO2 Photocatalysis
Published on: October 26, 2015
G Kevin Hyde1, S Michael Stewart, Giovanna Scarel
1Department of Chemical and Bimolecular Engineering, North Carolina State University, Raleigh, NC, USA.
Abstract:
TiO₂ films may be used to alter the wettability and hemocompatibility of cellulose materials. In this study, pure and stoichiometric TiO₂ films were grown using atomic layer deposition on both silicon and cellulose substrates. The films were grown with uniform thicknesses and with a growth rate in agreement with literature results. The TiO₂ films were shown to profoundly alter the water contact angle values of cellulose in a manner dependent upon processing characteristics. Higher amounts of protein adsorption indicated by blurry areas on images generated by scanning electron microscopy were noted on TiO₂ -coated cellulose acetate than on uncoated cellulose acetate. These results suggest that atomic layer deposition is an appropriate method for improving the biological properties of hemostatic agents and other blood-contacting biomaterials.